Assessment of Marginal Adaptation and Internal Fit of 3D-Printed Versus Milled Dental Crowns: An In Vitro Study

Main Article Content

Waleed Abdullah Alamri

Abstract

Background: Marginal adaptation and internal fit are parameters that have become increasingly important in the discussion of the biological and mechanical durability of a fixed restoration. Although additive manufacturing, such as 3D printing of a definitive crown, is now the clinical standard for restorations, the fit of additive manufacturing compared to subtractive milling continues to be debated.
The aim of this investigation is to compare the marginal gap and internal fit (axial and occlusal) of 3D-printed and milled monolithic hybrid-ceramic crowns.
Methods: 30 crowns in total were made using one standard master die from one CAD design and divided into two groups (n = 15); crowns milled from pre-polymerized hybrid-ceramic blocks (Group M) and crowns manufactured by DLP 3D printing from a ceramic filled hybrid resin (Group P). Fit was measured with the digital silicone replica technique and 3D superimpositions. Shapiro-Wilk, independent-samples t-tests, Cohen's d, and Fisher's exact test were used for statistical analysis at a threshold of α = 0.05.
Results: The mean value of marginal gap was 64.3 ± 6.2 µm in Group M and 46.9 ± 7.8 µm in Group P, with a mean difference of 17.4 µm (95% CI 12.1–22.7, p < 0.001). The internal fit was smaller in Group P (62.4 ± 6.1 µm vs. 77.2 ± 5.4 µm, p < 0.001). All crowns had a marginal gap value below the 120-µm threshold, which has been cited as a standard in the literature.
Conclusions: Under the conditions of the present in vitro study design, both manufacturing workflows achieved clinically acceptable fit; however, crowns fabricated with 3D printing had significantly lower marginal and internal gaps.

Article Details

Section
Articles