Comparative Evaluation of Fracture Resistance of Different CAD/CAM Restorative Materials Used for Posterior Teeth: An In Vitro Study

Main Article Content

Hamdan Hameed S. Almohammadi

Abstract

Background: Monolithic CAD/CAM crowns are widely used for posterior teeth, yet the fracture resistance of recent ceramic, glass-ceramic and hybrid materials after simulated aging remains incompletely compared.
Objective: To compare the fracture resistance of four CAD/CAM materials for posterior crowns before and after thermo mechanical aging.
Methods: The median fracture loads of ceramic crowns cemented on the epoxy-resin dies (n = 10) were (mean ± standard deviation): 2170 ± 298 N (24 h in water), 2557 ± 305 N (tc + ml).
Results: The median fracture loads of ceramic crowns cemented on human molar specimens (n = 10) were: 680 ± 523 N (24 h in water), 853 ± 465 N (tc + ml). There were significant differences between ceramic materials. Fracture loads (kd) of the crowns after tc + ml were significantly higher for all materials in comparison to the crowns cemented on the epoxy-resin dies.
The fracture load was significantly affected by material (F(3, 72) = 25.63, p < 0.001, partial η 2 = 0.52). The aged LDS (2680 ± 360 N) and ZLS crowns (2410 ± 330 N) had a significantly higher fracture load than PICN (1850 ± 270 N) and LDS also had a higher fracture load than RNC (2150 ± 300 N). The fracture load was reduced by ageing by between 6.1 – 8.0% for all materials (p = 0.017), but there was no interaction with material. There were more catastrophic failures with the glass-ceramics and more repairable fractures with the hybrid materials, with 75% of failures repairable for the hybrids.
Conclusion: In this in vitro study, all tested materials failed to the forces previously reported in the literature for the posterior occlusal forces after simulated 5-year aging; Lithium-based glass-ceramics provided higher load capacity and hybrid materials provided more favorable failure modes.