The Effect of Different Surface Treatments on the Bond Strength of Zirconia-Based Dental Restorations: A Systematic Review
Main Article Content
Abstract
Background: Yttria-stabilized tetragonal zirconia polycrystalline (Y-TZP) ceramics lack a glass matrix to allow conventional hydrofluoric acid etching. Formation of a reliable adhesive interface between a zirconia restoration and resin cement is necessary for clinical success.
Objective: To systematically review and meta-analyze the effects of mechanical, chemical and combined surface treatment protocols on shear bond strength (SBS) and microtensile bond strength (µTBS) of zirconia ceramics bonded to resin luting cements.
Methods: An extensive search was performed in Pub Med/MEDLINE, Scopus, Web of Science, and Google Scholar following the specifications of PRISMA 2020 for studies from 2020 to 2025. 15 studies which fit the high standards of inclusion criteria (see below) such as measurement of surface treatments, the quantitative measurements of SBS/µTBS and the utilization of artificial aging were selected for this review.
Results: The untreated controls revealed poor bonding values (4.5-9.4 MPa). Airborne-particle abrasion (APA) had yielded intermediate initial values of all bond strengths (18.5-24.1 MPa). Either APA or tribochemical silica coatings combined with 10-Methacryloyloxydecyl Dihydrogen Phosphate (10-MDP) systems produced the lowest and degraded bond strengths after the hydrolytic and/or thermal challenge (31.4-42.5 MPa, P < 0.0001). The new advanced non-thermal atmospheric plasma, hot-acid etching and LiSi Connect systems revealed potential achievers.
Conclusion: The use of APA or tribochemical coating for the micromechanical roughening, with 10-MDP chemical primers, is recommended as the gold standard clinical protocol for zirconia luting.